0
RESEARCH PAPERS

Enhancement of Fatigue Crack Growth and Fracture Resistance in Ti-6Al-4V and Ti-6Al-6V-2Sn Through Microstructural Modification

[+] Author and Article Information
G. R. Yoder, L. A. Cooley, T. W. Crooker

Engineering Materials Division, Naval Research Laboratory, Washington, D.C.

J. Eng. Mater. Technol 99(4), 313-318 (Oct 01, 1977) (6 pages) doi:10.1115/1.3443546 History: Received December 21, 1976; Revised April 27, 1977; Online August 17, 2010

Abstract

Significant enhancement in fatigue crack propagation resistance and plane strain fracture toughness was obtained in commercial purity Ti-6Al-4V and Ti-6Al-6V-2Sn through microstructural modification. Alloys studied were in the form of 25.4 mm-thick plate with interstitial oxygen contents of 0.20 and 0.17 weight percent, respectively. Heat treatments were chosen to provide widely varied microstructures; these included a mill anneal, recrystallization anneal and a beta anneal. The most beneficial heat treatment for improving these crack tolerance properties was found to be the beta anneal. However, the beta anneal resulted in yield strength reductions of 9 to 14 percent, from levels associated with the original mill anneal. The recrystallization anneal provided significant enhancement of plane strain fracture toughness and marginal improvement in fatigue crack propagation resistance with negligible loss of yield strength.

Copyright © 1977 by ASME
Your Session has timed out. Please sign back in to continue.

References

Figures

Tables

Errata

Discussions

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related Journal Articles
Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In