The Coefficient of Thermal Expansion of a Super Invar-Ta16W18O94 Composite

[+] Author and Article Information
C. N. Chu, N. Saka, N. P. Suh

Laboratory for Manufacturing and Productivity, Massachusetts Institute of Technology, Cambridge, MA 02139

J. Eng. Mater. Technol 108(3), 270-274 (Jul 01, 1986) (5 pages) doi:10.1115/1.3225880 History: Received April 14, 1985; Online September 15, 2009

Abstract

The coefficient of thermal expansion (CTE) of a hot pressed Ta16 W18 O94 which was produced from Ta2 O5 and WO3 powders was found to be −1.52×10−6 K−1 in the temperature range 180–330 K. Using the Ta16 W18 O94 and Super Invar powders, 50:50 volume percent metal-ceramic composites were made by the powder metallurgy techniques. When the mixture of constituent powders was hot pressed at 1123 K for 10 minutes, a CTE of 1.1 × 10−6 K−1 was obtained in the temperature range 140–420 K.

Copyright © 1986 by ASME
Your Session has timed out. Please sign back in to continue.

References

Figures

Tables

Errata

Discussions

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related Journal Articles
Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In